I'm still way down on the slope of the learning curve when it comes to new materials. Trying different things is interesting, and great when they work out. This was not one of those times.
I bought these intending to use them on my F-4B build and ended up not using them. They've been sitting there in my rack saying "use us".
So I did.
I found it hard to get full coverage without puddling. It is not that my brush was spitting blobs, but that is what it looked like. I think the effect was similar to surface tension, causing thick and thin spots. The contrast of silvers is definitely too strong here, I could work with that and tone it down as I applied more. but the pebble effect was getting frustrating.
Here's a better example of what I was seeing.
That is not the fault of surface-prep, unless one bottle of this product cannot be applied on top of another. This is an example of the darker silver on top of the lighter silver. The piece above was me quitting, so the top color is not fully applied. Yeah I see the hairs too, I had given up at this point.
Same effect, less zoom, and this one was a full coat.
This one does not have the darker silver, but shows the same effect again, even with heavy application. Unacceptable!
Now they are soaking in stripper. Will try again with a different paint. Think I'll search YouTube for tips on that product, hate to throw it away.